SnO2 thin films grown by atomic layer deposition using a novel Sn precursor

Min Jung Choi, Cheol Jin Cho, Kwang Chon Kim, Jung Joon Pyeon, Hyung Ho Park, Hyo Suk Kim, Jeong Hwan Han, Chang Gyoun Kim, Taek Mo Chung, Tae Joo Park, Beomjin Kwon, Doo Seok Jeong, Seung Hyub Baek, Chong Yun Kang, Jin Sang Kim, Seong Keun Kim

Research output: Contribution to journalArticlepeer-review

37 Citations (Scopus)

Fingerprint

Dive into the research topics of 'SnO2 thin films grown by atomic layer deposition using a novel Sn precursor'. Together they form a unique fingerprint.

Chemistry

Medicine and Dentistry

Material Science