Enhancement of a cyclic endurance of phase change memory by application of a high-density C15(Ge21Sb36Te43) film

J. H. Park, S. W. Kim, J. H. Kim, D. H. Ko, Z. Wu, D. Ahn, D. H. Ahn, J. M. Lee, S. B. Kang, S. Y. Choi

Research output: Contribution to journalArticlepeer-review

11 Citations (Scopus)

Abstract

The lower cyclic endurance of Phase Change Memory (PCM) devices limits the spread of its applications for reliable memory. The findings reported here show that micro-voids and excess vacancies that are produced during the deposition process and the subsequent growth in sputtered carbon-doped GeSbTe films is one of the major causes of device failure in PCM with cycling. We found that the size of voids in C15(Ge21Sb36Te43) films increased with increasing annealing temperature and the activation energy for the growth rate of voids was determined to be 2.22 eV. The film density, which is closely related to voids, varies with the deposition temperature and sputtering power used. The lower heat of vaporization of elemental Sb and Te compared to that for elemental Ge and C is a major cause of the low density of the film. It was possible to suppress void formation to a considerable extent by optimizing the deposition conditions, which leads to a dramatic enhancement in cyclic endurance by 2 orders of magnitude in PCM devices prepared at 300°C-300W compared to one prepared at 240°C-500W without change of compositions.

Original languageEnglish
Article number025013
JournalAIP Advances
Volume6
Issue number2
DOIs
Publication statusPublished - 2016 Feb 1

Bibliographical note

Publisher Copyright:
© 2016 Author(s).